• Low viscosity, easy impregnation of reinforcement materials.• Long pot life (2 hours for 100 ml at ambient), ample processing time allowsproduction of big objects.
• High temperature resistance (glass transition temperature) after ambient cure:60 °C, after post-cure at 100:120 °C.
• Excellent mechanical and dynamic properties after ambient cure with potentialfor even higher properties after post-cure at elevated temperatures.
• Also laminates show outstanding mechanical and dynamic properties. Thissystem is qualified by the Luftfahrtbundesamt (German Aircraft Authority) for theproduction of gliders.